1993-4-1 Cobalt-nickel separation: the extraction of cobalt (II) and nickel (II) by Cyanex 301, Cyanex 302 and Cyanex 272. Hydrometallurgv 32: 365-372. Cyanex 301, Cyanex 302
The selective separation of cobalt from acidic media, containing both equimolar and nonequimolar mixtures of cobalt and nickel, was examined by supported liquid
2016-1-12 The separation of cobalt from nickel in aqueous solution has always been a problem for hydrometallurgy. Their ad-jacent positions in transition metal series in the
2013-12-13 The separation of cobalt from Ni(OH) 2 positive material of spent NiMH batteries can be realized by a reduction and dissolution process, in which Co 3+ ions in the
Extraction and separation of nickel and cobalt from saprolite laterite ore were studied by using a method of microwave-assisted hydrothermal leaching and chemical
2021-2-16 A complete separation of nickel and cobalt was claimed, with the nickel depositing as metal at the cathode and the cobalt as peroxide at the anode. Two tests were
Zinc–cobalt slag, a hazardous waste from hydrometallurgical zinc smelting, is an important secondary source of cobalt; however, the separation of zinc and cobalt
Cobalt and nickel both have the same density, so it seems gravity separation which works based on the difference between density of materials is not a proper method.
2013-7-24 Separation or fractional recovery of each metal and. 4. Recovery of metals by electrolysis, precipitation, or crystallization. In the third step, separation of
When cobalt and nickel co-exist, they have to be separated from one another before the titrimetric or electrolytic methods can be employed. Most of the methods of separation of cobalt from nickel are based on3-4-5 the selective adsorption from hydrochloric acid solution of the chloro-complex of cobalt on a strongly basic anion-exchanger.
Spent lithium batteries contain valuable metals such as cobalt, copper, nickel, lithium, etc. After pretreatment and recovery of copper, only cobalt, nickel and lithium were left in the acid solution. Since the chemical properties of cobalt and nickel are similar, separation of cobalt
2009-4-1 Separation of cobalt and nickel from aqueous solutions has been a problem for hydrometallurgists due to their adjacent positions in transitional metal series in periodic table, which results in similar aqueous chemical behavior. Both the metals exist as divalent hexahydrated ions in dilute aqueous solutions.
2021-2-16 A complete separation of nickel and cobalt was claimed, with the nickel depositing as metal at the cathode and the cobalt as peroxide at the anode. Two tests were made with an electrolyte prepared from 8.2 grams of nickel sulfate, 0.5 gram of cobalt sulfate, 7.0 grams of potassium sulfate, and 0.3 gram of potassium dichromate per liter.
Extraction and separation of nickel and cobalt from saprolite laterite ore were studied by using a method of microwave-assisted hydrothermal leaching and chemical deposition.
The selective separation of cobalt from acidic media, containing both equimolar and nonequimolar mixtures of cobalt and nickel, was examined by supported liquid membranes using Alamine 336 as
2012-7-4 Cobalt in the raffinate exists in the Co(III) state. Therefore, model aqueous solutions containing 0.2 g/L Zn or 0.2 g/L Co were prepared by dissolving ZnSO4 or (Co(NH3)6·Cl3 in 60 g/L NH3, 60 g/L CO2 solution and investigated for separation of Zn
After leaching and removal of the impurities, the solution contains cobalt, magnesium, manganese and nickel. Solvent extraction is a hydrometallurgical technique used in the separation of metals
Separation of cobalt and nickel was investigated using a 4-stage countercurrent mixer-settler cascade, employing 2-ethylhexyl phosphonic acid mono-2-ethylhexyl ester as the extractant.
2017-8-11 Solid-liquid separation followed by precipitation of magnesium and manganese with monoammonium phosphate. Partial removal of ammonia from the clarified leach liquor. Coextraction of nickel and copper with LIX 64N in Kermac 470B in staged mixer-settler operations. Reduction of Co III in the raffinate to Co II in a cobalt
2021-2-16 A complete separation of nickel and cobalt was claimed, with the nickel depositing as metal at the cathode and the cobalt as peroxide at the anode. Two tests were made with an electrolyte prepared from 8.2 grams of nickel sulfate, 0.5 gram of cobalt sulfate, 7.0 grams of potassium sulfate, and 0.3 gram of potassium dichromate per liter.
Extraction and separation of nickel and cobalt from saprolite laterite ore were studied by using a method of microwave-assisted hydrothermal leaching and chemical deposition.
After leaching and removal of the impurities, the solution contains cobalt, magnesium, manganese and nickel. Solvent extraction is a hydrometallurgical technique used in the separation of metals
2012-7-4 Cobalt in the raffinate exists in the Co(III) state. Therefore, model aqueous solutions containing 0.2 g/L Zn or 0.2 g/L Co were prepared by dissolving ZnSO4 or (Co(NH3)6·Cl3 in 60 g/L NH3, 60 g/L CO2 solution and investigated for separation of Zn
Separation of cobalt and nickel from sulfate media was investigated, using a extraction system of 30% 2-ethylhexyl phosphonic acid mono-2-ethylhexyl ester (P507)+15% trioctyl/decylamine (N235)+55%
2013-7-7 Extraction and separation of nickel and cobalt from saprolite laterite ore were studied by using a method of microwave-assisted hydrothermal leaching and chemical deposition. The effects of leaching temperature and time on the extraction efficiencies of Ni2+ and Co2+ were investigated in detail under microwave conditions. It is shown that the extraction efficiencies of Ni2+ and Co2+ from the
2018-3-12 4 confirmed the cobalt can be extracted by [P 66614]Cl in the form of CoCl4 2−.22,25,27 Wellens et al.29 also presented experimental results of a continuous flowsheet for Co–Ni separation
2017-8-11 Solid-liquid separation followed by precipitation of magnesium and manganese with monoammonium phosphate. Partial removal of ammonia from the clarified leach liquor. Coextraction of nickel and copper with LIX 64N in Kermac 470B in staged mixer-settler operations. Reduction of Co III in the raffinate to Co II in a cobalt
2020-9-14 Mawson’s flagship is the 100%-owned Rajapalot gold-cobalt project, located just south of the Arctic Circle in Finnish Lapland.At Rajapalot the Company has made a significant greenfield discovery and on 26 August 2021 published an updated Inferred Mineral Resource. an updated resource estimation was completed by Eemeli Rantala, AFRY P.Geo, Ville-Matti Seppä, AFRY EurGeol of Finland
Its Co/Ni separation performance is superior to MEXTRAL 507P and Cyanex 272. Its ΔpH0.5 of Co and Ni was 1.9. At saponification ratio of 40%, the βCo/Ni of USTB-1 reached to 1.05×10⁴, while